MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman AVALON® 90 AB Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Performance Features: AVALON® injection molding products are trusted worldwide to deliver:
  • Outstanding flex performance
  • Excellent slip resistance
  • Perfect surface definition
  • Transparency and translucency
  • Oil resistance
  • Fast cycle times
  • Outstanding abrasion and scratch resistance
  • Perfect color match with masterbatches
  • Rubber-like look and feel
  • Excellent bonding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ISO 868
Hardness, Shore D 4444ISO 868
Tensile Strength at Break 32.0 MPa4640 psiISO 37
Elongation at Break 450 %450 %ISO 37
100% Modulus 8.00 MPa
@Strain 100 %
1160 psi
@Strain 100 %
ISO 37
300% Modulus 16.0 MPa
@Strain 300 %
2320 psi
@Strain 300 %
ISO 37
Flexural Modulus 0.0420 GPa6.09 ksiISO 178
Tear Strength 115 kN/m656 pliISO 34B
Abrasion 3535mm3; ISO 4649
 
Descriptive Properties
Ross Flex-10°C, BS 5131

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane
Huntsman AVALON® 80 AB Thermoplastic Polyurethane
Huntsman AVALON® 95 AB Thermoplastic Polyurethane
Huntsman AVALON® 650 B Thermoplastic Polyurethane
Huntsman AVALON® 65 DE Thermoplastic Polyurethane

PHUQ172 / 159545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.