MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® B3 GM 10/20 1 XL (4366) PA 6 Dry, 10/20% Glass/Mineral Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: AKROMID® Lite and AKROMID® XtraLite bridge the gap between polypropylene and polyamide. In comparison to polypropylene, AKROMID ® Lite and AKROMID® XtraLite display a superior surface quality, enhanced mechanical properties and higher heat resistance. In comparison to PA6 compounds, AKROMID ® Lite and AKROMID® XtraLite score higher in terms of lower density, lower volume price, superior flowability, reduced moisture absorption and enhanced notched impact strength. The objective of the AKROPLASTIC developers was to create a technical polyamide compound with a lower density while maintaining the typical properties of polyamide.

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ISO 1183
Filler Content 30 %30 %ISO 1172
Moisture Absorption 1.4 %
@Temperature 70.0 °C
1.4 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inISO 294-4
Spiral Flow 73.0 cm28.7 inCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 88.0 MPa12800 psi5 [mm/min]; ISO 527-2
Tensile Stress at Strain  25.0 MPa
@Strain 2 %,
Temperature 120 °C
3630 psi
@Strain 2 %,
Temperature 248 °F
Aged at 70°C, 62% RH for 500 hrs
 25.0 MPa
@Strain 10 %,
Temperature 120 °C
3630 psi
@Strain 10 %,
Temperature 248 °F
Aged at 70°C, 62% RH for 500 hrs
 27.0 MPa
@Strain 6.0 %,
Temperature 120 °C
3920 psi
@Strain 6.0 %,
Temperature 248 °F
Aged at 70°C, 62% RH for 500 hrs
 30.0 MPa
@Strain 1 %,
Temperature 80.0 °C
4350 psi
@Strain 1 %,
Temperature 176 °F
Aged at 70°C, 62% RH for 500 hrs
 45.0 MPa
@Strain 3 %,
Temperature 80.0 °C
6530 psi
@Strain 3 %,
Temperature 176 °F
Aged at 70°C, 62% RH for 500 hrs
 47.0 MPa
@Strain 5.0 %,
Temperature 80.0 °C
6820 psi
@Strain 5.0 %,
Temperature 176 °F
Aged at 70°C, 62% RH for 500 hrs
 60.0 MPa
@Strain 1 %,
Temperature 23.0 °C
8700 psi
@Strain 1 %,
Temperature 73.4 °F
Aged at 70°C, 62% RH for 500 hrs
 80.0 MPa
@Strain 2 %,
Temperature 23.0 °C
11600 psi
@Strain 2 %,
Temperature 73.4 °F
Aged at 70°C, 62% RH for 500 hrs
 95.0 MPa
@Strain 3 %,
Temperature 23.0 °C
13800 psi
@Strain 3 %,
Temperature 73.4 °F
Aged at 70°C, 62% RH for 500 hrs
 100 MPa
@Strain 1 %,
Temperature -30.0 °C
14500 psi
@Strain 1 %,
Temperature -22.0 °F
Aged at 70°C, 62% RH for 500 hrs
 145 MPa
@Strain 2 %,
Temperature -30.0 °C
21000 psi
@Strain 2 %,
Temperature -22.0 °F
Aged at 70°C, 62% RH for 500 hrs
Elongation at Break 3.4 %3.4 %5 [mm/min]; ISO 527-2
Tensile Modulus 5.10 GPa740 ksi1 [mm/min]; ISO 527-2
Charpy Impact Unnotched  4.30 J/cm²
@Temperature -30.0 °C
20.5 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 4.60 J/cm²
@Temperature 23.0 °C
21.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 208 °C406 °FHDT/B; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 165 °C329 °FHDT/A; ISO 75
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Nozzle Temperature 260 - 275 °C500 - 527 °F
Zone 1 220 - 280 °C428 - 536 °F
Zone 2 220 - 280 °C428 - 536 °F
Zone 3 220 - 280 °C428 - 536 °F
Zone 4 220 - 280 °C428 - 536 °F
Melt Temperature 260 - 280 °C500 - 536 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time <= 2.00 hour<= 2.00 hour
Hold Pressure 30.0 - 80.0 MPa4350 - 11600 psi
Back Pressure 50.0 MPa7250 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKRO161 / 182748

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.