MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe Lescalloy® HP 9-4-30 VAC-ARC ; 13.5 in RCS Billet Size High Strength Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: LESCALLOY HP 9-4-30 VAC-ARC steel is a low alloy, high strength steel with a high nickel and cobalt content to promote toughness. The alloy has been designed to have high hardenability, good weldability and excellent fracture toughness. It is typically used in the 220/240,000 psi (1517/1655 MPa) tensile strength range. Lescalloy HP 9-4-30 VAC-ARC steel is produced by the consumable electrode vacuum arc remelting process to provide optimum cleanliness and preferred ingot structure.

Normalized at 927°C; Austenitized at 829°C for .5 hour

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.280 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 511" from quench end; Jominy End Quench Hardenability
 511/2" from quenched end; Jominy End Quench Hardenability
 521/8" from quenched end; Jominy End Quench Hardenability
Tensile Strength, Ultimate 229 - 230 ksi
Tensile Strength, Yield 1260 - 1300 MPa
@Strain 0.2 %
Elongation at Break 14 - 14.7 %
Reduction of Area 45.9 - 50.3 %
Fracture Toughness 143 MPa-m½
Charpy Impact 27.0 J
@Temperature -54.0 °C
V-notch
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.3 µm/m-°C
@Temperature 20.0 - 427 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.30 %
Chromium, Cr 1.0 %
Cobalt, Co 4.5 %
Iron, Fe 85.2 %
Manganese, Mn 0.30 %
Molybdenum, Mo 1.0 %
Nickel, Ni 7.5 %
Silicon, Si 0.10 %
Vanadium, V 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe Lescalloy® AF 1410 VIM-VAR ; 6 in High Strength Alloy Steel
Latrobe Lescalloy® 300M - HS VAC-ARC High Strength Alloy Steel
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties
Latrobe Lescalloy® 35NCD16 VAC-ARC High Strength Alloy Steel
Latrobe Lescalloy® 4340 VAC-ARC ; 3.5" round High Strength Alloy Steel

NTIMK043 / 19390

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.