MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Toray PMC CFRT® TL-6000, 2 Layer Thermoplastic Composite Laminate
Categories: Polymer; Thermoplastic

Material Notes: Toray PMC CFRT® (TL-6000) is a reinforced thermoplastic composite that blends the benefits of a thermoplastic polymer matrix with woven carbon fibers for enhanced performance. Within the product range, 2 layer (MOD1, 2L), 3 layer (3L), or 4 layer (4L) products are available, all ultra-thin, lightweight, and resilient. This material can be drilled, ground, polished and adjusted after being formed with a heated gun. TL-6000 has a smooth high-gloss finish and transparent surface to show woven carbon fiber.

Features:

  • High strength and stiffness
  • High mechanical properties of “Thin & Light” (TL) laminates
  • Carbon fiber weave shown with a high-gloss and smooth finish
  • Choice of 2, 3, or 4 multilayers available
  • Core option available as MOD1 or with 4L
Product Type And Composition: CFRT® (Continuous Fiber Reinforced Thermoplastic) composite with carbon fiber and modified Polymethylmethacrylate (acrylic) resin

Typical Applications:

  • Orthosis knee and ankle bracing

Information provided by Toray Performance Materials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/cc
Thickness 1980 - 2410 microns
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 310 MPa
@Thickness 2.15 mm
Flexural Modulus 16.5 GPa
@Thickness 2.15 mm
 
Descriptive Properties
Flexural Rigidity1410 N-cm2.15 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTORAY8070 / 265468

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.