MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChenGuang EOCN-200 O-Cresol Novolac Epoxy Resin (EOCN)
Categories: Polymer; Thermoset; Epoxy

Material Notes: Main Applications: Mainly used as adhesives of encapsulating materials (epoxy molding plastics) for integrated circuits (LSI, VLSI, etc.), electronic components (diode, triode, etc.), and weak electric products (VTR, OP, etc.).
  • Modified by unsaturated acid, the EOCN vinyl ester resin owns both the main chain of EOCN and unsaturated double bond, so that it integrates the excellent solidifying properties and adhesiveness of EOCN, and the fast-curing and photocurable capability of unsaturated ester. These features make it a preferable material to manufacture GFRP products that require excellent resistance to heat and corrosion and to be used as a photo-sensitive resin in the application of printing ink .
  • Used as adhesives, coatings and laminated material for the applications that have special requirements for heat resistance, anti-corrosion and insulation.Properties and technical information: In addition to the general crosslinking performance of epoxy resin, EOCN features exceptional properties compared to ordinary epoxy resins. With the same softening point of 65-75 oC, the epoxy value of EOCN reaches 0.48-0.50eq/100g, while only 0.20eq/100g for the ordinary one. This fact means that its crosslinking points are 2.5 times more than usual, and its highlycrosslinked net with three-dimensional structure would be easily forming. With the phenolic framework additionally, the solidified products have excellent properties of heat stability, mechanical strength, electric insulation, waterproofness, low moisture absorption, resistance to chemicals, and higher glass transfer temperature Tg.

    Information provided by ChenGuang Research Institute of Chemical Industry

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Thermal PropertiesMetricEnglishComments
    Softening Point 70.0 - 75.0 °C158 - 167 °F
     
    Descriptive Properties
    AppearanceColorless or amber transparent particles, no mechanical impurities
    Content<1200 ppmSaponifiable chloride
     <300 ppmInorganic chloride
     195 - 205 g/eqEpoxy equivalence
    Volatility<0.2%110°C, 3hr

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    PCHENGU092 / 255691

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.