Characteristic: - Excellent abrasion resistance
- Outstanding smoothness
- High gloss
- High surface tension
- Does not exclude Varnish
- Good solvent resistance
- Good sliding properties
- Goyenchem-WF102 Micronized wax affordable, giving products with high added value
Applications: - Suitable for heat set inks and web offset printing inks
- Apply on water based liquid inks, but must use a high speed stirring apparatus so that the average dispersion
- Suitable for solvent (gravure and letterpress) ink
Information provided by Go Yen Chemical |