MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Melos Mecoline I RDX 1229 F Radiation cross-linkable non-halogen flame retardant polyolefin compound
Categories: Polymer; Thermoplastic

Material Notes: Radiation cross-linkable non-halogen flame retardant polyolefin compound

Compound class: Insulation / sheathing

Compound category: RDX

Flame retardant: ATH

Standards: SAE J1128 GXL; SAE J1127 SGX; SAE J1128 SXL; SAE J1127 STX; SAE J1128 TXL; HMC ES 91110-05; JASO D608 AESSXF; JASO D608 AEXF

Typical applications: An e-beam radiation cross-linkable, halogen-free low smoke compound, offering good mechanical and electrical properties.

Features: Flame retardant; Halogen-free; Low smoke; Oil resistant; Abrasion resistant; High temperature resistant; Flexible; Flexible at low temperatures

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccpressed plaques; DIN EN ISO 1183-1A
pH >= 4.7Corrosivity; IEC 60754-2
Melt Flow 3.0 g/10 min
@Load 10.0 kg,
Temperature 150 °C
DIN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52pressed plaques; DIN ISO 7619-1
Tensile Strength >= 10.0 MPaextruded tapes; IEC 60811-501
 15.0 MPacross-linked plaques or tapes, 50kGy; IEC 60811-501
Elongation at Break 200 %cross-linked plaques or tapes, 50kGy; IEC 60811-501
 230 %extruded tapes; IEC 60811-501
 10 %
@Temperature 200 °C,
Time 900 sec
Hot set test, Residual, 0.2 Mpa; IEC 60811-507
 20 %
@Temperature 200 °C,
Time 900 sec
Hot set test, under load, 0.2 Mpa; IEC 60811-507
 
Electrical PropertiesOriginal ValueComments
Insulation Resistivity 1.00e+12 Megaohm/1000 m
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 - 180 °CTool
 180 °CMaximum mass temperature
Zone 1 130 - 140 °C
Zone 2 135 - 145 °C
Zone 3 145 - 155 °C
Zone 4 150 - 160 °C
Zone 5 155 - 165 °C
Adapter Temperature 160 - 170 °C
Head Temperature 165 - 175 °C
Drying Temperature 60.0 - 70.0 °C
Dry Time 4.00 - 6.00 hour
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) 27 %ASTM D 2863 A
 
Descriptive Properties
Cold bend testNo crackswinding after 3hr at -40°C, HMC ES 91110-05
Conductivity=2.0 µS/mmpressed plaques, IEC 60754-2
Heat tests<0.5%Thermal shrinkage (1hr @ 100°C), HMC ES 91110-05
 No breakdownThermal overload (30 minutes @ 200°C), HMC ES 91110-05
Main burning properties<15 secFlame test, HMC ES 91110-05
 0Halogen content, IEC 754-1
Toxicity index<3NES 713

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMELOS032 / 296139

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.