MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Palm Labs Adhesives Turbo Fuse Series 130PR PLASTIC & RUBBER (100 Viscosity) Rapid Bonding Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130PR PLASTIC & RUBBER’S advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performance has been tested with a variety of materials, and is recommended for a multitude of applications, especially on plastics and rubbers. The fast curing qualities make it especially desirable in high speed industrial production and is ideal for use in applications that require an easily handled medium viscosity adhesive. Because of the 100 viscosity, it works especially well in close to medium fitting applications such as unfinished metal to metal bonding, metal to rubber, and rubber to rubber.

Part Numbers for this data: 04-130PR, 05-130PR, 06-130PR, 10-130PR, 15-130PR, 20-130PR, 25-130PR, 30-130PR, 35-130PR

Soluble in Acetone, MEK, Amide, Methylene Chloride

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 123-31-9
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccLiquid State
Viscosity 90 - 110 cPLiquid State
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 725 - 1450 psiCured; ASTM D1002/DIN 53283
 870 - 1310 psiCured; ASTM D1002/DIN 53283
 1160 - 2030 psiCured; ASTM D1002/DIN 53283
 1450 - 2180 psiCured; ASTM D1002/DIN 53283
 1450 - 2180 psiCured; ASTM D1002/DIN 53283
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 625 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CASTM D696
Thermal Conductivity 0.100 W/m-KASTM C177
Maximum Service Temperature, Air 180 °FCured State
Softening Point 160 - 170 °FCured State
Minimum Service Temperature, Air -65.0 °FCured State
Flash Point 160 - 200 °FLiquid State (Tagliabue closed cup)
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 MonthLiquid State
 
Descriptive Properties
AppearanceClear liquidLiquid State
 Clear-HardCured State
Base compound (Resin)Surface Insensitive Ethyl CyanoacrylateLiquid State
Chemical Resistance75% Initial Strength RetainedGasoline at 22°C, at 1000hrs
 80% Initial Strength RetainedGasoline at 22°C, at 500hrs
 85% Initial Strength RetainedIsopropanol at 22°C, at 500hrs
 85% Initial Strength RetainedIsopropanol at 22°C, at 1000hrs
 90% Initial Strength RetainedMotor Oil at 40°C, at 500hrs
 90% Initial Strength RetainedMineral Spirit at 22°C, at 500hrs
 90% Initial Strength RetainedMotor Oil at 40°C, at 1000hrs
 90% Initial Strength RetainedMineral Spirit at 22°C, at 1000hrs
Gap Fill0.20 mmCured State

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPALML020 / 135174

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.