MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical NBR 6850 High Acrylonitrile Polymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: NBR 6850 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6850 is a non staining, medium mooney, and medium high acrylonitrile polymer designed for easy processing, high productivity and excellent elastic properties. NBR 6850 offers very low mold fouling, fast cure, and high resilience. NBR 6850 is a high mooney version of NBR 6840.

Applications: NBR 6850 is recommended to use in wide range of general purpose applications including injection molded o-rings, calendared belting, extruded hose and sponge.

CAS No: 9003-18-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/cc
Volatiles 0.30 %
Mooney Viscosity 50
@Temperature 100 °C
ML 1+4
Ash <= 1.0 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 47
@Treatment Temp. 25.0 °C,
Time 259000 sec
Aged fuel C
 71
@Treatment Temp. 145 °C,
Time 1190 sec
Cured
 72
@Treatment Temp. 100 °C,
Time 259000 sec
Aged ASTM D #3 Oil
 77
@Treatment Temp. 100 °C,
Time 259000 sec
Circulating Oven Aging
 77
@Treatment Temp. 100 °C,
Time 259000 sec
Aged ASTM D #1 Oil
Tensile Strength at Break 14.0 MPa
@Treatment Temp. 25.0 °C,
Time 259000 sec
Aged fuel C
 18.6 MPa
@Treatment Temp. 145 °C,
Time 1190 sec
Cured
 19.3 MPa
@Treatment Temp. 100 °C,
Time 259000 sec
Aged ASTM D #3 Oil
 19.6 MPa
@Treatment Temp. 100 °C,
Time 259000 sec
Aged ASTM D #1 Oil
 19.8 MPa
@Treatment Temp. 100 °C,
Time 259000 sec
Circulating Oven Aging
 28.9 MPa
@Treatment Temp. 145 °C,
Time 2990 sec
cured; ASTM D412
Elongation at Break 355.3 %
@Treatment Temp. 25.0 °C,
Time 259000 sec
Aged fuel C
 381.1 %
@Treatment Temp. 100 °C,
Time 259000 sec
Aged ASTM D #1 Oil
 383.7 %
@Treatment Temp. 100 °C,
Time 259000 sec
Circulating Oven Aging
 386 %
@Treatment Temp. 100 °C,
Time 259000 sec
Aged ASTM D #3 Oil
 406 %
@Treatment Temp. 145 °C,
Time 1190 sec
Cured
 492 %
@Treatment Temp. 145 °C,
Time 2990 sec
cured; ASTM D412
300% Modulus 159 kg(f)/cm²
@Treatment Temp. 145 °C,
Time 2990 sec
cured; ASTM D412
Rebound 49.1 %
@Temperature 30.0 °C
Abrasion 0.3265AKRON
Compression Set 20.4 %
@Temperature 100 °C,
Time 259000 sec
160°C x 30 min. Cured)
 
Descriptive Properties
Bound AN Content (%)34
ColorLight Tan
ComponentsHAF (IRB#7)40 phr, ASTM D3187
 NBR 6850100 phr, ASTM D3187
 Stearic Acid1 phr, ASTM D3187
 Sulfur1.5 phr, ASTM D3187
 TBBS0.7 phr, ASTM D3187
 ZnO3 phr, ASTM D3187
Compound RecipeAntioxidant(3-C)1 phr
 Antioxidant(RD)2 phr
 Carbon Black(SRF)80 phr
 CZ2 phr
 NBR 6850100 phr
 Plasticizer(DOP)10 phr
 Stearic Acid1 phr
 Sulfur0.5 phr
 TT1 phr
 Zinc Oxide5 phr
Rheometer0.8 mints1, 160°C x 12 min, 1° Arc, MDR
 1.2 mint'50, 160°C x 12 min, 1° Arc, MDR
 1.6 mint'90, 160°C x 12 min, 1° Arc, MDR
 2.2 lb-inML, 160°C x 12 min, 1° Arc, MDR
 29.4 lb-inMH, 160°C x 12 min, 1° Arc, MDR
Volume Swell (%)-2.5Aged ASTM D #3 Oil (100°C x 72hrs)
 42.1Aged fuel C (23°C x 72hrs)
 -6.6Aged ASTM D #1 Oil (100°C x 72hrs)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical NBR 6230 High Acrylonitrile Polymer
LG Chemical NBR 6840 High Acrylonitrile Polymer
LG Chemical NBR 6280 High Acrylonitrile Polymer
LG Chemical NBR 3250 High Acrylonitrile Polymer
LG Chemical NBR 6250 High Acrylonitrile Polymer

PLAY738 / 148748

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.