MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Northstar Polymers MPS-F04A Hand-Mixable Flexible Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and ambient pressure. It requires minimum tooling for a small production or short runs. These properties are ideal in small scale productions for custom foam applications such as custom seating, padding, and cushioning.

Generally, lower density grade foams are softer than higher density foams. For firmer foam quality, 8 or 6 pound-per-cubic foot formulas are recommended.

The free-rise density of the foam is 4.5 pounds per cubic foot, and the cell structure is designed to be open-cell. This is an MDI base water-blown polyester/polyether hybrid system, and it does not use flammable or ozone-layer-depleting auxiliary blowing agents.

Examples for Applications:

  • Molded Upholstery Parts
  • Custom Seating, Padding, and Cushioning Parts
  • Custom Packaging of Impact/Vibration-Sensitive Items
  • Prototyping

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0705 g/cc0.00255 lb/in³Free Rise Density
 0.0785 g/cc0.00284 lb/in³Typical Compression Density
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 30 - 4530 - 45
Tensile Strength 0.207 MPa30.0 psi
Elongation at Break 138 %138 %
Compressive Strength  0.0124 MPa
@Strain 25 %
1.80 psi
@Strain 25 %
 0.0241 MPa
@Strain 50 %
3.50 psi
@Strain 50 %
Rebound 31 %31 %Bashore Rebound
Tear Strength 0.701 kN/m4.00 pliSplit Tear Resistance
 
Processing PropertiesMetricEnglishComments
Processing Temperature 21.1 - 32.2 °C70.0 - 90.0 °FPrepolymer Temperature
 21.1 - 32.2 °C70.0 - 90.0 °FCuring Agent Temperature
Mold Temperature 37.8 - 54.4 °C100 - 130 °F
Cure Time  19.8 - 30.0 min
@Temperature 43.3 °C
0.330 - 0.500 hour
@Temperature 110 °F
De-mold Time
 60.0 min
@Temperature 82.2 °C
1.00 hour
@Temperature 180 °F
Complete Cure Cycle
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Complete Cure Cycle
Pot Life 0.170 - 0.250 min0.170 - 0.250 min
 
Descriptive Properties
Curing AgentPPB-023
PrepolymerMSA-018
Weight Ratio1:1.27Prepolymer to Curing Agent Ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mearthane Durethane™ M DM-630A Foam Polyurethane
Mearthane Durethane™ M DM-650A Foam Polyurethane
Mearthane Durethane™ M DM-640A Foam Polyurethane
Mearthane Durethane™ F DF-255A Closed Cell Foam Polyurethane
Overview of materials for Thermoset Polyurethane Foam, Unreinforced

PNORTH890 / 162606

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.