MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Albis Plastics ABS 01A FR 05 Unreinforced  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Amorphous Acrylonitrile Butadiene Styrene Terpolymer (ABS)

Characteristics: Flame Retardant: Balanced Properties (Mechanical, Impact and Heat), High Flow

Applications: Computer, Monitor and Printer Housings, Microwave Components

Processing: Injection Molding (Melt Temperature: 320-425°F, Mold Temperature: 100-140°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ASTM D792
Melt Flow 4.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9898ASTM D785
Tensile Strength at Break 40.2 MPa5830 psiASTM D638
Tensile Strength, Yield 39.2 MPa5690 psiASTM D638
Flexural Yield Strength 59.8 MPa8670 psiASTM D790
Flexural Modulus 2.35 GPa341 ksiASTM D790
Izod Impact, Notched 1.56 J/cm2.92 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °FASTM D648
Vicat Softening Point 86.0 °C187 °FASTM D1525
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
Albis Internal Test
 
Processing PropertiesMetricEnglishComments
Melt Temperature 160 - 218 °C320 - 424 °FInjection
Mold Temperature 38.0 - 60.0 °C100 - 140 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Albis Plastics ABS 01A FR01 Unreinforced
A. Schulman Diamond ABS VP-11
LNP Stat-Loy® A- FR Acrylonitrile Butadiene Styrene
IRPC Polimaxx Porene AN520 Acrylonitrile Butadiene Styrene
IRPC Polimaxx Porene AN510 Acrylonitrile Butadiene Styrene

PZA1A18 / 21613

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.