MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Wacker® E 37 Silicone Resin Emulsion
Categories: Polymer; Thermoset; Silicone

Material Notes: WACKER® E 37 is a nonionic/anionic oil-in-water emulsion whose active ingredient combines the benefits of both polydimethylsiloxanes and silicone resins. WACKER® E 37 can be readily incorporated into cold-stirred formulations.

Application: WACKER® E 37 is used primarily in the polishes and release agent sectors. Used in polishes, e. g. car polishes, it enhances the detergent and weathering resistance of the treated surface as well as increases depth of image and gloss. Since WACKER® E 37 is supplied as an oil-in-water emulsion, it is also eminently suitable for formulating extremely efficient, aqueous release agents, e. g. for the processing of microcellular PUR foams.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 40 %
Particle Size 150 µm
pH 5.0
 
Descriptive Properties
Appearancemilky

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3003/30 A/B Liquid Silicone Rubber
Overview of materials for Silicone Elastomer, for Thermal Management
NuSil CF2-4721 Silicone Resin
Hippe SI GC 21 Woven Glass Cloth Reinforced Silicone Resin - Round, Rolled Tube
Hippe SI GC 201 Woven Glass Cloth Reinforced Silicone Resin - Sheet

PWACK9747 / 205276

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.