MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optimized injection molding performance. This product is available in natural, grey & black colors as standard and can be made in other specific colors upon request.

Benefits: This product offers excellent flame retardancy properties (UL 94, 5VA, GWIT) combined with excellent processing, mechanical and electrical performance. It can withstand temperatures of 160°C for over 6000 hours and has a UL F1 rating for weatherability resistance.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: This product is ideally suited for industrial controls, power distribution or appliance applications such as MCBs and contactors. The long term thermal performance of this grade also make it ideal for under-the-bonnet Auto applications.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccISO 1183/A
Water Absorption 0.83 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0050 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
Melt Flow 27 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO/FDIS 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPaASTM D638
 142 MPaISO 527 Type 1A
Tensile Stress at Strain 30.0 MPa
@Strain 1 %,
Temperature 140 °C
 37.0 MPa
@Strain 1 %,
Temperature 100 °C
 41.0 MPa
@Strain 2 %,
Temperature 140 °C
 45.0 MPa
@Strain 1 %,
Temperature 60.0 °C
 50.0 MPa
@Strain 4 %,
Temperature 140 °C
 60.0 MPa
@Strain 2 %,
Temperature 100 °C
 70.0 MPa
@Strain 4 %,
Temperature 100 °C
 80.0 MPa
@Strain 1 %,
Temperature -40.0 °C
 80.0 MPa
@Strain 1 %,
Temperature 23.0 °C
 80.0 MPa
@Strain 2 %,
Temperature 60.0 °C
 85.0 MPa
@Strain 4 %,
Temperature 60.0 °C
 122 MPa
@Strain 2 %,
Temperature 23.0 °C
 140 MPa
@Strain 2 %,
Temperature -40.0 °C
Elongation at Break 2.0 %ISO 527 Type 1A
 2.8 %ASTM D638
Tensile Modulus 9500 MPaISO 527 Type 1A
Flexural Strength 195 MPaASTM D790
Flexural Modulus 8300 MPaASTM D790
Izod Impact, Notched (ISO) 95.0 kJ/m²ISO 180/1eA
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 65.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 30.0 kV/mmIEC 60243
Comparative Tracking Index 550 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 262 °CASTM D3417
 263 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 260 °CISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 240 °CISO 75/Af
 246 °CASTM D648
UL RTI, Electrical 65.0 °C
@Thickness 0.400 mm
 130 °C
@Thickness 0.800 mm
 130 °C
@Thickness 1.00 mm
 130 °C
@Thickness 1.50 mm
 130 °C
@Thickness 3.00 mm
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 0.400 mm
 105 °C
@Thickness 0.800 mm
 105 °C
@Thickness 1.00 mm
 115 °C
@Thickness 1.50 mm
 115 °C
@Thickness 3.00 mm
Flammability, UL94 V-0
@Thickness 0.800 mm
1210
 V-0
@Thickness 1.60 mm
1210
 V-0
@Thickness 3.20 mm
1210
Oxygen Index 33 %ISO 4589
Glow Wire Ignition Temperature 775 °C
@Thickness 1.60 mm
ISO 60695-2-13
 775 °C
@Thickness 3.20 mm
ISO 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
ISO 60695-2-12
 960 °C
@Thickness 3.20 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 260 - 275 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone275-280°C
Mixing Zone280-285°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, Conditioned
Domo TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, Conditioned
Domo TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, DRY
Domo TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, DRY
Domo Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant

PRHOD722 / 137953

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.