MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nabaltec APYMAG® 30S Magnesium Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these products is of growing importance.

If processing temperatures exceed 200°C, APYMAG® should be used. It is preferable for applications which are very sensitive to processing parameters, like viscosity. When using in thermoplastics, good mechanical and flame retardancy can be achieved.

Information provided by Nabaltec.

Key Words: MgOH
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 g/cc
Density 2.40 g/cc
Brightness 90 %
@Wavelength 457 nm
Whiteness; Elrepho
Oil Absorption 19 %(ml/100 g)
Moisture Absorption at Equilibrium 0.50 %
Loss On Ignition 31 %
Particle Size 12 µmMedian; Laser Diffraction
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2857 ohm-cm
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 300 °C
 
Descriptive Properties
Magnesium Hydroxide (%)90
Sieve Analysis0.2%> 45 µm
Stearic Acid (%)0.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex APEX® 75-9351A-102 Flexible Polyvinyl Chloride
NAECO® ELKON® 30S Silver Tungsten contact material ASTM B631
Kleerdex Vinyloy™ 102 Acrylic/PVC Thermoplastic Sheet
Fainplast Compounds PMP 102 Flexible PVC, Extrusion Modified with PU

CNABAL23A / 159810

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.