MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omnia Plastica PE 1000 - Polyethylene 1000
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Polyethylene with a molecular weight of ± 1000,000 with excellent impact strength. PE 1000 is less rigid and has a higher shock resistance than the low molecular weight polyethylene and it is therefore more suitable for applications subject to continuous shocks.

Features:

  • Shock resistance, good even at low temperatures High chemical resistance typical of the polyolefins
  • High abrasion resistance
  • Low friction coefficient
  • Low specific gravity
  • Easy machinability
  • Colour: natural
Weak Point:

Compared to the engineering plastics it has lower thermal and mechanical properties: tensile stress, flexural and compressive strength, etc. Compared to low molecular weight PE, it is less rigid.

Application:

  • Food contact : physiologically inert, it is approved for food contact by the most important standards. Thanks to this feature, it is widely used for components in food machinery, pumps for liquid food etc.
  • Chemical: thanks to the high resistance to acids and alkali it is used for components in the chemical industry
  • Electrical: very good dielectric properties, weatherproof
  • Mechanical: the low friction coefficient and its non hygroscopicity make it suitable for use as a bearing or mechanical parts with low loads, even when operating in water.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccISO.1183 DIN.53479
Moisture Absorption at Equilibrium 0.00 %50% relative humidity
Water Absorption at Saturation 0.00 %23°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 60dry sample; ISO2039.2
Ball Indentation Hardness 40.0 MPaISO2039.1 DIN.53456
Tensile Strength at Break 22.0 MPaISO.527 DIN.53455
Elongation at Break 200 %ISO.527 DIN.53455
Tensile Modulus 0.780 GPaISO.527 DIN.53455
Compressive Strength 3.00 MPa1% strain over 1000 hours; ISO.899 DIN.53444
Charpy Impact Unnotched NB7.5 J; ISO.R179 DIN.53453
Charpy Impact, Notched 8.00 J/cm²ISO179/3C DIN.53453
Coefficient of Friction, Dynamic 0.30on dry ground steel; load =0.05MPa; speed =0.6 m/s
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmISO.93 DIN.53482
Dielectric Constant 2.3
@Frequency 1e+6 Hz
ISO.250 DIN.53483
Dielectric Strength 45.0 kV/mmISO.243 DIN.53481
Dissipation Factor 0.0040
@Frequency 1e+6 Hz
ISO.250 DIN.53483
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
@Temperature 23.0 - 60.0 °C
Thermal Conductivity 0.400 W/m-KDIN.52612
Melting Point 130 °C
Maximum Service Temperature, Air 80.0 °CContinuous; 5000 hours based on a tensile stress of 50% at 23° C.
 100 °Cshort period, no load
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO.75 DIN.53461
Minimum Service Temperature, Air -50.0 °Cimpact conditions and heavy loads not considered
Flammability, UL94 HB
Oxygen Index 18 %ISO.4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer
Hippe PE 1000 Polyethylene
Westlake Plastics Lennite® Biocompatible Implant Grade UHMW-PE
A. Schulman ComAlloy Hiloy® 515 Polycarbonate, Carbon Fiber Reinforced

POMNIA36 / 55626

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.