MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Alphawool® Unifelt Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Alphawool ® Unifelt™ is made of polycrystalline bulk fibers bonded with an organic binder which burns out on exposure to 180-200°C (356-392°F). Alphawool ® Unifelt™ demonstrates excellent flexibility with excellent dimensional resilience after compression and makes utilization of the felt or cut pieces very easy to handle compared to rigid products. Alphawool ® Unifelt™ is supplied in a wide range of thickness minimum 6mm to a maximum 50mm (combining light weight, high heat resistance, and low thermal conductivity). Typical applications: Expansion joints , Furnace lining, Gaskets

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 0.0900 g/cc>= 0.00325 lb/in³
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0600 W/m-K
@Temperature 400 °C
0.416 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C201
 0.0900 W/m-K
@Temperature 600 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C201
 0.140 W/m-K
@Temperature 800 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 1470 °F
ASTM C201
 0.210 W/m-K
@Temperature 1000 °C
1.46 BTU-in/hr-ft²-°F
@Temperature 1830 °F
ASTM C201
 0.290 W/m-K
@Temperature 1200 °C
2.01 BTU-in/hr-ft²-°F
@Temperature 2190 °F
ASTM C201
 0.340 W/m-K
@Temperature 1300 °C
2.36 BTU-in/hr-ft²-°F
@Temperature 2370 °F
ASTM C201
 0.390 W/m-K
@Temperature 1400 °C
2.71 BTU-in/hr-ft²-°F
@Temperature 2550 °F
ASTM C201
Shrinkage <= 5.0 %
@Temperature 1600 °C,
Time 86400 sec
<= 5.0 %
@Temperature 2910 °F,
Time 24.0 hour
isothermal
 
Component Elements PropertiesMetricEnglishComments
Al2O3 93 - 96 %93 - 96 %
Loss on Ignition(%) <= 5.0 %<= 5.0 %
Other 0.00 - 2.0 %0.00 - 2.0 %
SiO2 3.0 - 5.0 %3.0 - 5.0 %
 
Descriptive Properties
Colorwhite / tan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool A Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 80 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 3000 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 2600 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic

CMORF70137 / 203435

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.