MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hannam Chemical Hanalac 750 ABS, General Purpose
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: FDA Approved. Good combination of impact strength, rigidity, gloss, heat resistance, processability, and thermal stability. May be injection molded. Its broad range of applications include: electronic home appliances (TVs, fans, mixers, switch panels), calculators and cash registers, telephones.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 4.5 g/10 minASTM D1238G
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ASTM D785
Tensile Strength, Ultimate 47.0 MPaASTM D638
Elongation at Break 30 %ASTM D638
Flexural Yield Strength 64.0 MPaASTM D790
Flexural Modulus 2.34 GPaASTM D790
Izod Impact, Notched 2.50 J/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 85.0 °CHeat Distortion Temp
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °CASTM D648
Vicat Softening Point 95.0 °CASTM D1525
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hannam Chemical Hanalac 710 ABS
Delrin Delrin® 500AF POM-SF20
Omnia Plastica ABS Acrylonitrile-butadiene-styrene
Hannam Chemical Hanalac 780 ABS, High Flow
Chi Mei Polylac® PA-758 ABS - Transparent

PLAH03 / 49815

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.