DuPont™ Elvax® CE9619-1 is an extrudable ethylene-vinyl acetate copolymer resin concentrate available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. This EVA resin concentrate is intended to be let down with compatible resins and in that intended use may be safely used as articles or components of articles intended for use in contact with food as provided in FDA regulation 21CFR 177.1350 - "Ethylene-vinyl acetate copolymers," subject to the extraction limitations on the finished food contact articles as specified in the regulation. Additives: 73% Elvax® 3170 based resin, antiblock 20%, slip 7%. Information provided by DuPont™ This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition. |