MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Extir® AM 5000 AE Flame Retardant Expanded Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Extir AM 5000 AE is an HBCD-free flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir AM 5000 AE is suitable for production of low-medium density blocks for the thermal insulation sector.

Applications: Extir AM 5000 AE is used mainly in the construction sector where, for legislative or safety reasons, the use of a flame retardant material is required. Typical applications are: blocks, especially for external thermal insulation, low density elasticized blocks for impact sound absorption (Trittschall), void formers, trough formers and culvert formers cut from block, blocks or slabs for road foundations and civil construction.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.0590 - 0.0630 g/cc0.00213 - 0.00228 lb/in³
Density >= 0.0100 g/cc>= 0.000361 lb/in³continuous pre-expander after two expansions
 >= 0.0130 g/cc>= 0.000470 lb/in³Discontinuous pre-expander.
 >= 0.0150 g/cc>= 0.000542 lb/in³Continuous pre-expander after one expansion
 0.0110 - 0.0200 g/cc0.000397 - 0.000723 lb/in³Normal Density Range
Particle Size 900 - 1600 µm900 - 1600 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENF9889 / 265619

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.