MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kaowool 333-E Paper
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Kaowool 333-E expandable paper is an intumescent material produced from a unique blend of Kaowool high-purity ceramic fibers, special additives, and organic binders in a special paper-making process. At maximum expansion which occurs at approximately 1200°F (649°C), the paper expands up to 400% of its thickness. This results in the 333-E Paper being an excellent candidate for high-temperature gaskets and seals. During heat up and expansion, there will be some additional out-gassing of the intumescent additives.

Like all the other high-quality Kaowool paper products, this specialty paper is noted for its excellent flexibility, outstanding handling characteristics, and high-insulating value.

Features:

  • Low thermal conductivity and heat storage
  • Easily die cut for high temperature gasketing and seals
  • Thickness expansion up to 400%
  • Applications:

  • All purpose high temperature gasketing and sealing
  • Expansion joint insulation
  • Fireplace catalytic converter gasketing
  • Fire protection
  • Industrial furnace seals
  • Aluminum filter bowl gasketing
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.240 - 0.288 g/cc0.00867 - 0.0104 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate 0.0345 - 0.0689 MPa5.00 - 10.0 psiFired
     0.517 - 0.689 MPa75.0 - 100 psi
     
    Thermal PropertiesMetricEnglishComments
    Melting Point 1760 °C3200 °F
    Maximum Service Temperature, Air 1150 °C2100 °F
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 42 - 45 %42 - 45 %
    Carbon, C 5.0 - 10 %5.0 - 10 %
    SiO2 48 - 50 %48 - 50 %
     
    Descriptive Properties
    Organic Binder content6-10%
    Other Element Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    CTHERM252 / 2572

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.