MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Domo TECHNYL® A 218 V25 NAT BA PA66, 25% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.

Available in: Asia Pacific

Product Applications: TECHNYL® A 218 V25 NAT BA is recommended for molding parts exposed to high temperatures and in contact with oils and greases. Bearing housings are a typical example for which this formulation is suitable. This product is approved by major bearing manufacturers. This product is available in natural.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183/A
Water Absorption 0.90 %
@Temperature 23.0 °C,
Time 86400 sec
0.90 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/in
Linear Mold Shrinkage, Transverse 0.0085 cm/cm0.0085 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 170 MPa24700 psiASTM D638
Elongation at Break 3.5 %3.5 %ASTM D638
Flexural Strength 260 MPa37700 psiASTM D790
Flexural Modulus 7.50 GPa1090 ksiASTM D790
Izod Impact, Notched (ISO) 85.0 kJ/m²40.4 ft-lb/in²ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 27.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
15.0 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 262 °C504 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FASTM D648
Flammability, UL94 HB
@Thickness 0.800 - 3.20 mm
HB
@Thickness 0.0315 - 0.126 in
1210
Oxygen Index 23 %23 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Feed Temperature 260 - 270 °C500 - 518 °F
Front Barrel Temperature 280 - 290 °C536 - 554 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY

PRHOD630 / 137861

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.