MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NuSil MED1-4855 Specialty Liquid Silicone Rubber - Unrestricted Medical Use
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Description: Liquid silicone rubbers, or LSRs, are elastomer systems reinforced with silica. They contain functional polymers of lower average molecular weight and viscosity when compared to high consistency rubbers (HCRs). They are typically supplied as two-component systems and formulated in a 1:1 mix ratio. Because their consistency is akin to petroleum jelly, they are often pumped with injection molding equipment to form molded components such as o-rings, gaskets, valves, seals, and other precision molded parts.

Important Properties of Adhesives: LSRs are designed for liquid injection molding (LIM) processes which may utilize single or multi-cavity molds, or for overmolding processes. Originally designed for automated systems, they are developed with high volume applications in mind and benefit from their high strength. Features of liquid silicone rubbers include the following:

  • Ideal for high throughput manufacturing
  • Platinum cure system—no post cure required
  • Typical work time in excess of 72 hours
  • Cure rapidly at elevated temperatures
  • Easily pigmented using NuSil color masterbatches
Comments: Injection Molding Elastomer, Self Lubricating

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555Typical
 50 - 6050 - 60Certified
Tensile Strength at Break 5.50 MPa798 psiCertified
 7.60 MPa1100 psiTypical
Elongation at Break 250 %250 %Certified
 450 %450 %Typical
Tear Strength 21.9 kN/m125 pliCertified
 39.4 kN/m225 pliTypical
 
Processing PropertiesMetricEnglishComments
Extrusion Rate 150 g/min150 g/min
Cure Time 5.00 min
@Temperature 165 °C
0.0833 hour
@Temperature 329 °F
Working Life 1440 min
@Temperature 25.0 °C
1440 min
@Temperature 77.0 °F
 
Descriptive Properties
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Loctite® SpeedBonder™ 326 Fast Fixture Acrylic Bonding Adhesive
Cariflex IR0307 K Polyisoprene
Dow C6-570 LIQUID SILICONE RUBBER KIT
Dow Silastic® 7-6840 BIOMEDICAL GRADE LSR, KIT
Dow Silastic® 99-595-HC LIQUID SILICONE RUBBER KIT

PNUSIL297 / 142021

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.