MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Bamberger Polymers Bapolan® PS6450 Polystyrene, Injection Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Bapolan PS6450 is a high impact polystyrene injection molding resin which offers high impact strength, flexibility, shock resistance, gloss and processability. This product meets FDA standards for food contact applications.

Applications: Appliance housings, toys, industrial parts.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: High impact strength, flexibility, shock resistance, gloss and processability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D1505
Melt Flow 8.0 g/10 min8.0 g/10 min200°C/5000g; ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 1010ASTM D-785
Tensile Strength, Ultimate 22.1 MPa3210 psi2 in/min (50 mm/min); ASTM D-638
Elongation at Break 55 %55 %2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 2.41 GPa350 ksiSecant @ 1% strain; ASTM D-790
Izod Impact, Notched 0.960 J/cm1.80 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °FASTM D-648
Vicat Softening Point 93.0 °C199 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss 90 %90 %ASTM D-2457
 
Descriptive Properties
processInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBP3B340 / 20835

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.