MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Silver, CP Grade, Cold Drawn then Annealed at 100°C (212°F)
Categories: Metal; Nonferrous Metal; Precious Metal; Pure Element

Key Words: Silver, Ag
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 10.49 g/cc0.3790 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 300 MPa43500 psi
Elongation at Break 4.0 %4.0 %
Modulus of Elasticity 71.0 GPa10300 ksiTypical of CP silver.
Poissons Ratio 0.370.37
Shear Modulus 26.0 GPa3770 ksicalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000177 ohm-cm
@Temperature 20.0 °C
0.00000177 ohm-cm
@Temperature 68.0 °F
Temperature coefficient is .0041/°C 0-100°C.
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 105 J/g45.2 BTU/lb
CTE, linear  19.68 µm/m-°C
@Temperature 0.000 - 100 °C
10.93 µin/in-°F
@Temperature 32.0 - 212 °F
typical of CP silver
 20.0 µm/m-°C
@Temperature 0.000 - 250 °C
11.1 µin/in-°F
@Temperature 32.0 - 482 °F
estimated
 20.6 µm/m-°C
@Temperature 0.000 - 500 °C
11.5 µin/in-°F
@Temperature 32.0 - 932 °F
typical of CP silver
Specific Heat Capacity  0.234 J/g-°C
@Temperature 0.000 °C
0.0559 BTU/lb-°F
@Temperature 32.0 °F
 0.236 J/g-°C
@Temperature 100 °C
0.0564 BTU/lb-°F
@Temperature 212 °F
Thermal Conductivity 418.68 W/m-K2905.6 BTU-in/hr-ft²-°F
Melting Point 961.93 °C1763.5 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.055
@Temperature 700 °C
0.055
@Temperature 1290 °F
Reflection Coefficient, Visible (0-1) 0.900.90
 
Component Elements PropertiesMetricEnglishComments
Silver, Ag 100 %100 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Gold Alloy
Silver, Ag; Refined, ASTM 413 (UNS P07015)
Overview of materials for Palladium Alloy
Overview of materials for Molybdenum Alloy
Morgan Advanced Ceramics Nicusil™ Mac-Nicusil™ 8-WM Braze Alloy

MPAg05 / 12501

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.