MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Nextel™ DF-11 Woven Fabric 610
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.90 g/cc0.141 lb/in³
Permeability 2020[ft3/min/ft2], Air w/o sizing
Thickness 280 microns11.0 mil
Fiber Count 1670 dtex1500 denierroving
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 3100 MPa450000 psifilament 25.4mm
Tensile Modulus 379 GPa55000 ksifilament
Tear Strength 40.2 kN/m230 pliWarp, Breaking Strength w/o Sizing
 45.1 kN/m258 pliFill, Breaking Strength w/o Sizing
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 9.0
@Frequency 9.375e+9 Hz
9.0
@Frequency 9.375e+9 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 µm/m-°C
@Temperature 100 - 1100 °C
4.44 µin/in-°F
@Temperature 212 - 2010 °F
Melting Point 2000 °C3630 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.741.74
 
Component Elements PropertiesMetricEnglishComments
Al2O3 99 %99 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Nextel™ CFAMC Aluminum Matrix Composite
3M Nextel™ DF-19 Woven Fabric 610
3M Nextel™ AF-10 Aerospace Woven Fabric 312

PMM33019 / 167766

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.