MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Phenolic, Novolac, Flock Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Flock Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 - 1.45 g/ccAverage value: 1.41 g/cc Grade Count:7
Water Absorption 0.180 - 0.630 %Average value: 0.436 % Grade Count:7
Linear Mold Shrinkage 0.00300 - 0.00850 cm/cmAverage value: 0.00576 cm/cm Grade Count:7
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 63.0 - 91.0Average value: 77.7 Grade Count:7
Tensile Strength, Ultimate 36.0 - 55.7 MPaAverage value: 48.6 MPa Grade Count:7
Elongation at Break 0.710 - 1.00 %Average value: 0.817 % Grade Count:6
Modulus of Elasticity 6.90 - 8.27 GPaAverage value: 7.70 GPa Grade Count:6
Flexural Yield Strength 61.0 - 83.2 MPaAverage value: 74.2 MPa Grade Count:7
Flexural Modulus 6.20 - 7.72 GPaAverage value: 7.12 GPa Grade Count:7
Compressive Yield Strength 139 - 213 MPaAverage value: 175 MPa Grade Count:7
Poissons Ratio 0.300 - 0.350Average value: 0.338 Grade Count:4
Shear Modulus 2.56 - 3.00 GPaAverage value: 2.87 GPa Grade Count:4
Izod Impact, Notched 0.210 - 0.277 J/cmAverage value: 0.241 J/cm Grade Count:6
Charpy Impact, Notched 0.199 - 0.400 J/cm²Average value: 0.271 J/cm² Grade Count:7
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 6.38e+10 - 2.13e+12 ohm-cmAverage value: 5.65e+11 ohm-cm Grade Count:7
Dielectric Constant 4.50 - 6.60Average value: 5.14 Grade Count:7
Dielectric Strength 7.90 - 16.2 kV/mmAverage value: 11.1 kV/mm Grade Count:7
Dissipation Factor 0.0400 - 0.0760Average value: 0.0560 Grade Count:7
Arc Resistance 26.0 - 160 secAverage value: 110 sec Grade Count:7
Comparative Tracking Index 150 - 175 VAverage value: 168 V Grade Count:7
 
Thermal PropertiesOriginal ValueComments
CTE, linear 44.0 - 67.0 µm/m-°C
@Temperature 40.0 - 130 °C
Average value: 54.0 µm/m-°C Grade Count:3
Thermal Conductivity 0.370 - 0.400 W/m-K
@Temperature 100 - 100 °C
Average value: 0.385 W/m-K Grade Count:2
Maximum Service Temperature, Air 170 - 200 °CAverage value: 189 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 156 - 196 °CAverage value: 173 °C Grade Count:7
Flammability, UL94 HB - V-0Grade Count:7
Oxygen Index 24.2 - 27.1 %Average value: 25.7 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PEN-PET
Overview of materials for PEKK, Unreinforced
Overview of materials for PEKK, Reinforced
Overview of materials for PCTG Copolyester
Overview of materials for PCTA Polyester Alloy

O2719 / 78089

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.