MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC PPE reactive chemistries AP2001G
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: NORYL™ AP2001G polyol is a low molecular weight di-functional hydroxyl-terminated polyol based on polyphenylene ether (PPE). The incorporation of NORYL AP2001G polyol into a solid elastomer matrix may demonstrate structure-property benefits in traditional CAST polyurethane material formulations. Incorporating NORYL AP2001G polyol into these systems may: - Improve toughness and reduce abrasion - Increase tensile strength - Improve strain modulus and elongation - Maintain physical properties at elevated temperatures and after humid aging - Improve resistance to alkaline, acid, water and oil - Improve adhesion to steel

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 880 g/mol880 g/molHydroxy Equivalent Weight (HEW); SABIC method
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 140 °C284 °Fhalf width; SABIC method
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %SABIC method
 
Descriptive Properties
Physical FormPELLETSABIC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80005 / 287952

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.