MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPE ML-1690B BLK Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ML-1690B BLK is a general purpose designed for automotive interior applications. Sarlink ML-1690B BLK is a high hardness, medium density grade suitable for injection molding. This high flow TPE exhibits improved Moldability and surface appearance.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Filled; Good Mold Release; Good Moldability; Good Processability; High Flow; Medium Density; High Hardness

Uses: Automotive Applications; Automotive Interior Parts; General Purpose; Grommets

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO 1183
Viscosity 133 cP
@Shear Rate 206 1/s,
Temperature 200 °C
133 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 190 °C
24 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  90
@Time 15.0 sec
90
@Time 0.00417 hour
Injection Molded; ISO 868
 91
@Time 5.00 sec
91
@Time 0.00139 hour
Injection Molded; ISO 868
 92
@Time 1.00 sec
92
@Time 0.000278 hour
Injection Molded; ISO 868
 90.0
@Treatment Temp. 125 °C,
Time 15.0 sec
90.0
@Treatment Temp. 257 °F,
Time 0.00417 hour
Change in Air, 168 hr; ISO 888
 90.4
@Treatment Temp. 125 °C,
Time 1.00 sec
90.4
@Treatment Temp. 257 °F,
Time 0.000278 hour
Change in Air, 168 hr; ISO 888
 90.9
@Treatment Temp. 110 °C,
Time 15.0 sec
90.9
@Treatment Temp. 230 °F,
Time 0.00417 hour
Change in Air, 1008 hr; ISO 888
 90.9
@Treatment Temp. 125 °C,
Time 5.00 sec
90.9
@Treatment Temp. 257 °F,
Time 0.00139 hour
Change in Air, 168 hr; ISO 888
 91.5
@Treatment Temp. 110 °C,
Time 5.00 sec
91.5
@Treatment Temp. 230 °F,
Time 0.00139 hour
Change in Air, 1008 hr; ISO 888
 92
@Treatment Temp. 110 °C,
Time 1.00 sec
92
@Treatment Temp. 230 °F,
Time 0.000278 hour
Change in Air, 1008 hr; ISO 888
Tensile Strength at Break 8.07 MPa1170 psiAcross Flow, Type 1, 20 in/min; ISO 37
 10.1 MPa1460 psiFlow, Type 1, 20 in/min; ISO 37
 8.33 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
1210 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Type 1, Change in Air; ISO 188
 9.28 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
1350 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Type 1, Change in Air; ISO 188
 9.70 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
1410 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Flow, Type 1, Change in Air; ISO 188
 9.74 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
1410 psi
@Treatment Temp. 257 °F,
Time 168 hour
Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain  4.90 MPa
@Strain 100 %
711 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 6.17 MPa
@Strain 100 %
895 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 5.38 MPa
@Strain 100 %,
Treatment Temp. 110 °C
780 psi
@Strain 100 %,
Treatment Temp. 230 °F
Across Flow, Type 1, Change in Air, 1008 hr; ISO 188
 5.49 MPa
@Strain 100 %,
Treatment Temp. 125 °C
796 psi
@Strain 100 %,
Treatment Temp. 257 °F
Across Flow, Type 1, Change in Air, 6.61 in; ISO 188
 6.97 MPa
@Strain 100 %,
Treatment Temp. 110 °C
1010 psi
@Strain 100 %,
Treatment Temp. 230 °F
Flow, Type 1, Change in Air, 1008 hr; ISO 188
 7.10 MPa
@Strain 100 %,
Treatment Temp. 125 °C
1030 psi
@Strain 100 %,
Treatment Temp. 257 °F
Flow, Type 1, Change in Air, 168 hr; ISO 188
Elongation at Break 580 %580 %Flow, Type 1, 20 in/min; ISO 37
 590 %590 %Across Flow, Type 1, 20 in/min; ISO 37
 552 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
552 %
@Treatment Temp. 230 °F,
Time 1008 hour
Flow, Type 1, Change in Air; ISO 188
 560 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
560 %
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Type 1, Change in Air; ISO 188
 568 %
@Treatment Temp. 125 °C,
Time 605000 sec
568 %
@Treatment Temp. 257 °F,
Time 168 hour
Flow, Type 1, Change in Air; ISO 188
 642 %
@Treatment Temp. 125 °C,
Time 605000 sec
642 %
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 38.6 kN/m220 pliFlow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
 47.3 kN/m270 pliAcross Flow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
Compression Set  38 %
@Temperature 22.8 °C,
Time 79200 sec
38 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ISO 815
 62 %
@Temperature 70.0 °C,
Time 79200 sec
62 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ISO 815
 76 %
@Temperature 90.0 °C,
Time 252000 sec
76 %
@Temperature 194 °F,
Time 70.0 hour
Type 1; ISO 815
 100 %
@Temperature 125 °C,
Time 252000 sec
100 %
@Temperature 257 °F,
Time 70.0 hour
Type 1; ISO 815
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 193 °C340 - 380 °F
Middle Barrel Temperature 177 - 199 °C350 - 390 °F
Front Barrel Temperature 182 - 204 °C360 - 400 °F
Nozzle Temperature 188 - 210 °C370 - 410 °F
Melt Temperature 188 - 210 °C370 - 410 °F
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1116 / 237607

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.