MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nouryon Trigonox 125-W40 tert-Amyl peroxypivalate, 40% emulsion in water and methanol
Categories: Other Engineering Material

Material Notes: Trigonox 125-W40 (40% emulsion in water and methanol) is an initiator for (co)polymerization of vinyl chloride and vinylidene chloride.

CAS number: 29240-17-3

EINECS/ELINCS No: 64741-65-7

Applications: Polymerization of vinyl chloride: Trigonox 125-W40 can be applied as an initiator for the suspension polymerization of vinyl chloride in the temperature range between 50°C and 65°C. Trigonox 125-W40 may be used in combination with other initiators to increase reactor efficiency.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.888 g/cc
@Temperature -10.0 °C
0.0321 lb/in³
@Temperature 14.0 °F
Half-life  0.100
@Temperature 91.0 °C
0.100
@Temperature 196 °F
[hr]
 1.00
@Temperature 72.0 °C
1.00
@Temperature 162 °F
[hr]
 10.0
@Temperature 54.0 °C
10.0
@Temperature 129 °F
[hr]
Viscosity 200 - 1000 cP
@Temperature -10.0 °C
200 - 1000 cP
@Temperature 14.0 °F
Molecular Weight 188.3 g/mol188.3 g/mol
Storage Temperature -25.0 - -10.0 °C-13.0 - 14.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 25.0 °C77.0 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay39.0-41.0 %
Content (%)3.4Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1006 / 286529

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.