MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Bostik LVT-Lock™ Flooring Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Description: Bostik LVT-Lock™ is a solvent-free, single-component, water-based, acrylic adhesive specifically formulated for the installation of most resilient flooring. LVT-Lock™ is a 0-VOC formulation as calculated per SCAQMD Rule 1168. LVT-Lock™ is formulated using special acrylic polymer emulsions and tackifiers that enable either “wet-set” or “transitional pressure sensitive” installation methods. It displays tenacious early bond strength, and is specially formulated to be highly resistant to plasticizer migration and staining. LVT-Lock™ has been formulated to exhibit a unique combination of application properties including; excellent trowelability, fast tack/grab, low odor and easy clean up.

Key Features:

  • Rapid tacking
  • Bonds a wide variety of flooring
  • Plasticizer migration resistant

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³
Solids Content 68 %68 %
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
pH 5.0 - 9.05.0 - 9.0
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.3 °C>= 200 °F
 
Processing PropertiesMetricEnglishComments
Working Life 25.0 - 30.0 min25.0 - 30.0 min
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBOSTK039 / 191575

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.