MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

DuPont Mobility and Materials Betafill™ 10101 Polyoxypropylene Sealant
Categories: Polymer; Adhesive; Thermoset

Material Notes: One component, sprayable and moisture curing Polyoxypropylene (P-O-P) based seam sealant with permanent elasticity and good adhesion to various substrates.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 - 1.70 g/cc0.0397 - 0.0614 lb/in³ISO 845
Viscosity 5000 - 9000 cP5000 - 9000 cPHaake RU 20
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 47>= 47DIN 53505
Tensile Strength at Break 1.80 MPa261 psiISO 1798
Elongation at Break 250 %250 %ISO 1798
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air <= 80.0 °C<= 176 °F
 120 °C248 °FShort term in cured condition
Minimum Service Temperature, Air >= -40.0 °C>= -40.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 5.00 - 35.0 °C41.0 - 95.0 °F
Shelf Life 9.00 Month
@Temperature 5.00 - 25.0 °C
9.00 Month
@Temperature 41.0 - 77.0 °F
in unopened containers.
 
Descriptive Properties
BasisPOP Polyoxypropylene
ColorGray
Cure rate (mm), Minimum3after 24h
PolymerAdhesive
Regional AvailabilityEurope
 Near East/Africa
Skinning time15 - 35 Minutes.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDTF9012 / 254081

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.