MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Asahi Kasei Leona™ 14G33 Polyamide 66, Heat Stabilized, GF Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Enhanced strength and stiffness; with 33% GF. Superior heat aging resistance, fatigue resistance, and creep resistance.

Applications:Mechanical and electrical parts, engine mounts and other under-the-hood automotive parts

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccDry as Molded; ASTM D792
Density 1.39 g/ccDry as Molded; ISO 1183
Moisture Absorption at Equilibrium 1.7 %
@Temperature 23.0 °C
50% RH; ISO 62
 1.7 %
@Temperature 23.0 °C
50% RH
Linear Mold Shrinkage, Flow >= 0.0040 cm/cmAsahi Kasei
Linear Mold Shrinkage, Transverse >= 0.0080 cm/cmAsahi Kasei
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 75Conditioned at 50% RH; ISO 2039
 96Dry as Molded; ISO 2039
Hardness, Rockwell R 120Dry as Molded; ISO 2039
Tensile Strength at Break 143 MPaConditioned at 50% RH; ISO 527
 208 MPaDry as Molded; ISO 527
Tensile Strength 135 MPaConditioned at 50% RH; ASTM D638
 210 MPaDry as Molded; ASTM D638
Elongation at Break 4.0 %Dry as Molded; ISO 527
 6.0 %Conditioned at 50% RH; ISO 527
Tensile Modulus 7.80 GPaDry as Molded; ISO 527
 9.80 GPaConditioned at 50% RH; ISO 527
Flexural Strength 213 MPaConditioned at 50% RH; ISO 178
 302 MPaDry as Molded; ISO 178
Flexural Modulus 6700 MPaConditioned at 50% RH; ISO 178
 9600 MPaDry as Molded; ISO 178
Izod Impact, Notched 130 J/mDry as Molded; ASTM D256
 170 J/mConditioned at 50% RH; ASTM D256
Charpy Impact Unnotched 90.0 kJ/m²Dry as Molded; ISO 179
 97.0 kJ/m²Conditioned at 50% RH; ISO 179
Charpy Impact, Notched 13.0 kJ/m²Dry as Molded; ISO 179
 16.0 kJ/m²Conditioned at 50% RH; ISO 179
Taber Abrasion, mg/1000 Cycles 15Conditioned at 50% RH; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmDry as Molded; IEC 60093
Surface Resistance 1.00e+15 ohmDry as Molded; IEC 60093
Dielectric Strength 33.0 kV/mmDry as Molded; IEC 60243
Comparative Tracking Index 425 V
@Thickness 3.00 mm
Dry as Molded; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°CDry as Molded; ASTMD 696
Thermal Conductivity 0.300 W/m-KDry as Molded
Deflection Temperature at 0.46 MPa (66 psi) 260 °CDry as Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 250 °CDry as Molded; ISO 75
Flammability, UL94 HB
@Thickness 0.750 mm
Dry as Molded

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei Leona™ 14G15 Polyamide 66, Heat Stabilized, GF Reinforced
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
Celanese SO.F.TER Reblend® 4510 Unreinforced PC/ABS alloy
Kingfa MAC-501DY Modified PC/ABS Alloy
Kingfa PA6-RG30 Flame Retardant, 30% Glass Fiber Reinforced PA6

PASAHI8137 / 221164

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.