System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Asahi Kasei Leona™ 14G15 Polyamide 66, Heat Stabilized, GF Reinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
Material Notes:
Applications: Heater tanks, fuel injectors, ABS sensors, and other under-the-hood automotive parts
Information provided by Asahi Kasei Corp.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.25
g/cc
1.25
g/cc
Dry as Molded; ASTM D792
Density
1.25
g/cc
0.0452
lb/in³
Dry as Molded; ISO 1183
Moisture Absorption at Equilibrium
2.1 %
@Temperature 23.0 °C
2.1 %
@Temperature 73.4 °F
50% RH; ISO 62
2.1 %
@Temperature 23.0 °C
2.1 %
@Temperature 73.4 °F
50% RH
Linear Mold Shrinkage, Flow
>=
0.0070
cm/cm
>=
0.0070
in/in
Asahi Kasei
Linear Mold Shrinkage, Transverse
>=
0.012
cm/cm
>=
0.012
in/in
Asahi Kasei
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
71
71
Conditioned at 50% RH; ISO 2039
94
94
Dry as Molded; ISO 2039
Hardness, Rockwell R
120
120
Dry as Molded; ISO 2039
Tensile Strength at Break
73.0
MPa
10600
psi
Conditioned at 50% RH; ISO 527
107
MPa
15500
psi
Dry as Molded; ISO 527
Tensile Strength
79.0
MPa
11500
psi
Conditioned at 50% RH; ASTM D638
108
MPa
15700
psi
Dry as Molded; ASTM D638
Tensile Strength, Yield
77.0
MPa
11200
psi
Conditioned at 50% RH; ISO 527
Elongation at Break
2.5 %
2.5 %
Dry as Molded; ISO 527
11 %
11 %
Conditioned at 50% RH; ISO 527
Elongation at Yield
6.0 %
@Temperature 23.0 °C
6.0 %
@Temperature 73.4 °F
Conditioned at 50% RH; ISO 527
Tensile Modulus
3.60
GPa
522
ksi
Dry as Molded; ISO 527
5.80
GPa
841
ksi
Conditioned at 50% RH; ISO 527
Flexural Strength
116
MPa
16800
psi
Conditioned at 50% RH; ISO 178
162
MPa
23500
psi
Dry as Molded; ISO 178
Flexural Modulus
3.30
GPa
479
ksi
Conditioned at 50% RH; ISO 178
4.80
GPa
696
ksi
Dry as Molded; ISO 178
Izod Impact, Notched
0.490
J/cm
0.918
ft-lb/in
Dry as Molded; ASTM D256
0.590
J/cm
1.11
ft-lb/in
Conditioned at 50% RH; ASTM D256
Charpy Impact Unnotched
2.60
J/cm²
12.4
ft-lb/in²
Dry as Molded; ISO 179
3.80
J/cm²
18.1
ft-lb/in²
Conditioned at 50% RH; ISO 179
Charpy Impact, Notched
0.500
J/cm²
2.38
ft-lb/in²
Conditioned at 50% RH; ISO 179
0.600
J/cm²
2.86
ft-lb/in²
Dry as Molded; ISO 179
Taber Abrasion, mg/1000 Cycles
9.0
9.0
Conditioned at 50% RH; ASTM D1044
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
Dry as Molded; IEC 60093
Surface Resistance
1.00e+15
ohm
1.00e+15
ohm
Dry as Molded; IEC 60093
Dielectric Strength
26.0
kV/mm
660
kV/in
Dry as Molded; IEC 60243
Comparative Tracking Index
425
V
@Thickness 3.00 mm
425
V
@Thickness 0.118 in
Dry as Molded; IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear
40.0
µm/m-°C
22.2
µin/in-°F
Dry as Molded; ASTMD 696
Deflection Temperature at 0.46 MPa (66 psi)
260
°C
500
°F
Dry as Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
235
°C
455
°F
Dry as Molded; ISO 75
Flammability, UL94
HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
Dry as Molded
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Asahi Kasei Leona™ 14G33 Polyamide 66, Heat Stabilized, GF Reinforced
Kingfa PA66-RG301 Flame Retardant, 30% Glass Fiber Reinforced PA66
Kingfa PA6-RG30 Flame Retardant, 30% Glass Fiber Reinforced PA6
Kingfa PBT-RG301 Flame Retardant, 30% Glass Fiber Reinforced PBT
Kingfa PET-RG20 Flame Retardant, 20% Glass Fiber Reinforced PET
PASAHI8134 / 221161
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.