MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Manganese Brass, UNS C66700, H06 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: Extra Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding; Fair Suitability – Gas Shielded Arc Welding, Capacity for Being Hot Formed

Common Fabrication Processes: Bending; Blanking; Forming; Resistance Welding; Seam and Butt Welding; Spot Welded Components; Stamping

Typical uses: Resistance Weldable Brass Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.53 g/cc0.308 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 89
@Thickness 1.02 mm
89
@Thickness 0.0400 in
Hardness, Rockwell 30T 7575
Tensile Strength 607 MPa
@Thickness 1.02 mm
88000 psi
@Thickness 0.0400 in
Tensile Strength, Yield 586 MPa
@Thickness 1.02 mm
85000 psi
@Thickness 0.0400 in
0.2% Offset
Elongation at Break 4.0 %
@Thickness 1.02 mm
4.0 %
@Thickness 0.0400 in
Tensile Modulus 110 GPa16000 ksi
Machinability 30 %30 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000101 ohm-cm0.0000101 ohm-cm17% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 - 300 °C
11.1 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 8.07 W/m-K56.0 BTU-in/hr-ft²-°F
Melting Point 1050 - 1090 °C1920 - 2000 °F
Solidus 1050 °C1920 °F
Liquidus 1090 °C2000 °F
Annealing Point 499 - 704 °C930 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 727 - 849 °C1340 - 1560 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 68.5 - 71.5 %68.5 - 71.5 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.070 %<= 0.070 %
Manganese, Mn 0.80 - 1.5 %0.80 - 1.5 %
Zinc, Zn 26.8 - 30.7 %26.8 - 30.7 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC66700x4 / 293067

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.