Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of EPO-TEK® 320 that can be poured, potted or cast into shape.Information Provided by Epoxy Technology |