MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Proto Labs Titanium Grade 5 Ti-6Al-4V - DMLS
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Due to its light weight, high strength, and excellent high temperature and corrosion resistance, titanium is often used for aerospace applications. Proto Labs uses a high-grade Ti 6-4, making it an excellent choice for medical applications as well.

Information provided by Proto Labs.

Key Words: Direct Metal Laser Sintering; ASTM F2924-14; Ti-6-4; UNS R56400; Ti6Al4V; 3D Printing; Additive Manufacturing
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 40
Tensile Strength, Ultimate 172 ksi
Tensile Strength, Yield 164 ksi
@Strain 0.2 %
Elongation at Break 10 %
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 6.0 %
Titanium, Ti 90 %Nominal
Vanadium, V 4.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Ti-6Al-4V (Grade 5), Annealed Bar
Titanium Ti-6Al-4V (Grade 5), Annealed
Titanium Grade 2
Titanium Ti-6Al-4V (Grade 5), STA
TIMET TIMETALĀ® 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet

NPROTO995 / 232389

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.