STYRON™ A-TECH™ 1220 advanced technology polystyrene resin is a high impact, high modulus resin for extrusion thermoforming applications. The improved durability of this resin allows potential down-gauging and scrap reduction, as well as overall improvements in process efficiency.
Main Characteristics - Easy Processing
- Outstanding thermoform-ability
- High Modulus/Toughness Balanced
- Good Trim-ability
- Complies with U.S. FDA 21 CFR 177.1640
Applications - Packaging/Disposables
- Cold Drink Cups
- Plates/Bowls
- Portion Containers