MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2099 X 124790 B Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Fast-Cycle Nucleator - 68% Renewable Resource Content
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Nucleated for high heat exposure.  For detailed processing information regarding this, see the PLA Molding Guide on the RTP Company website.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D 792
Additive Loading 10 %10 %Primary Additive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 37.9 MPa5500 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Flexural Strength 65.5 MPa9500 psiASTM D 790
Flexural Modulus 3.45 GPa500 ksiASTM D 790
Izod Impact, Notched 1.87 J/cm
@Thickness 3.20 mm
3.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 71.1 °C160 °FASTM D 648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 171 - 193 °C340 - 380 °F
Mold Temperature 82.2 - 104 °C180 - 220 °F
Drying Temperature 54.4 °C
@Time 7200 - 21600 sec
130 °F
@Time 2.00 - 6.00 hour
Moisture Content 0.020 %0.020 %
Dew Point -40.0 °C-40.0 °F
Injection Pressure 55.2 - 103 MPa8000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2099 X 124790 A Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Fast Cycle Nucleator - 78% Renewable Resource Content
RTP Company RTP 2099 X 124790 F Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Fast-Cycle Nucleator - 53% Renewable Resource Content
RTP Company RTP 2099 X 121249 D Bio-Based Polylactic Acid (PLA); Standard Nucleator - Glass Fiber - 58% Renewable Resource Content
RTP Company RTP 2099 X 124790 C Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Standard Nucleator - 78% Renewable Resource Content
RTP Company RTP 2099 X 126216 C Bio-Based Polylactic Acid (PLA); Fast-Cycle Nucleator - Glass Fiber - 68% Renewable Resource Content

PQZUA19875 / 134732

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.