MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reynolds TASK® 14 (C-1520) Semi-Rigid Black Urethane Casting Resin
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: TASK™ 13 and TASK™ 14 are fast setting two-component urethanes that cure quickly to black semi-rigid plastics. TASK™ 13 has a pot life of 3 minutes and demold time of 20 minutes. TASK™ 14 offers a longer pot life (10 minutes) and demold time of 45 minutes. With a Shore value of 50D, these semi-rigid plastics are used for a variety of industrial applications including fast mold making, fast model duplication, prototyping, durable miniatures, black props and special effects, or making parts that are impact resistant. Fully cured castings are tough, durable and chemical resistant.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D-1475
Viscosity 800 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.0035 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ASTM D-2240
Hardness, Shore D 50ASTM D-2240
Tensile Strength, Ultimate 1800 psiASTM D-638
Elongation at Break 125 %ASTM D-638
 
Processing PropertiesOriginal ValueComments
Cure Time 45.0 minHandling Time
Pot Life 10.0 minASTM D-2471
 
Descriptive Properties
ColorBlack
Mix Ratio100A:120Bby weight
Specific Volume24.1[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN040 / 296741

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.