MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chambroad Petrochemicals PPS-GF30 30% Glass Fiber Reinforced, Polyphenylene sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler

Material Notes: Modified PPS Materials: Polyphenylene sulfide (PPS) resin has a simple molecular structure and is a heat-resistant crystal polymer of the unit consisting of an aromatic ring alternated with sulfur atoms. With a melting point of about 280°C, the resin has a high resistance to heat and reagents, and can extinguish automatically without adding flame retardants. Since PPS can replace metal or thermosetting resin, it is widely applied in the fields of car parts, electrical/electronic parts, housing facilities, OA, and precision equipment.

Application Field: Aerospace - Gun shells, helmets, corrosion-resistant and wear-resistant parts of warships and submarines, aircraft connectors, coil frames, and instrument panels.

Information provided by Shandong Chambroad Petrochemicals Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccISO 1183
Water Absorption 0.020 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0030 - 0.0080 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 169 MPaISO 527-1, 2
Elongation at Break 2.5 %ISO 527-1, 2
Tensile Modulus 13.5 GPaISO 527-1, 2
Flexural Strength 234 MPaISO 178
Flexural Modulus 12.0 GPaISO 178
Flexural Strain at Break 2.4 %ISO 178
Charpy Impact Unnotched 36.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²ISO 179/1eA
Coefficient of Friction, Dynamic 0.35b
Coefficient of Friction, Static 0.35b
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 26.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.0040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 - 45.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 266 °C
Flammability, UL94 V-0
@Thickness 0.750 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 300 - 340 °CBarrel
Mold Temperature 130 - 150 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHAMB017 / 318559

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.