MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Felix Compounds S50080 SEEPS based compound
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Applications: Extrusion

Information provided by Felix Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 - 0.980 g/cc0.930 - 0.980 g/ccASTM D792
Melt Flow <= 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
<= 1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 78 - 8278 - 82ASTM D2240
Tensile Strength >= 10.3 MPa>= 1500 psi500mm/min; ASTM D412
Elongation at Break >= 500 %>= 500 %500mm/min; ASTM D412
300% Modulus >= 8.27 MPa>= 1200 psi500mm/min; ASTM D412
Abrasion <= 150<= 150[mg-loss]; DIN 53516
Compression Set 23 - 27 %
@Temperature 70.0 °C,
Time 79200 sec
23 - 27 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395-B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 210 °C338 - 410 °FBarrel
Screw Speed 30 - 70 rpm30 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFELIX027 / 294762

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.