MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Indium Corp. Indalloy 200 Pure Gold
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Pure Element

Material Notes:

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 19.3 g/cc0.697 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 138 MPa20000 psi
Elongation at Break 39 - 45 %39 - 45 %2in.
Modulus of Elasticity 77.2 GPa11200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000230 ohm-cm0.00000230 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 °C
7.78 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.130 J/g-°C0.0311 BTU/lb-°FSolid
Thermal Conductivity 318 W/m-K
@Temperature 85.0 °C
2210 BTU-in/hr-ft²-°F
@Temperature 185 °F
Melting Point 1064 °C1947 °F
Solidus 1064 °C1947 °F
Liquidus 1064 °C1947 °F
 
Component Elements PropertiesMetricEnglishComments
Gold, Au 100 %100 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NNIN894 / 98103

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.