MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silicone-free; Suitable for vacuum; Stress resistant
Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine Tools

Information provided by Zedex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183
Water Absorption 0.050 %
@Temperature 23.0 °C
RMC 93%; DIN EN ISO 62
Moisture Absorption at Equilibrium 0.50 %DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 93DIN 53505
Hardness, Shore D 81DIN 53505
Ball Indentation Hardness 174 MPaDIN 2039
Tensile Strength at Break 84.0 MPaDIN EN ISO 527
Tensile Strength 110 MPaDIN EN ISO 527
Tensile Strength, Yield 81.0 MPaElastic Limit
 110 MPaDIN EN ISO 527
Tensile Stress at Strain 43.0 MPa
@Strain 1 %,
Time 3.60e+6 sec
DIN 53444
Elongation at Break 12.6 %
 12.6 %DIN EN ISO 527
Elongation at Yield 4.2 %Elastic Yield Point
 7.0 %DIN EN ISO 527
 7.0 %Elongation at Maximum Force; DIN EN ISO 527
Tensile Modulus 3600 MPaDIN EN ISO 527
Flexural Strength 126 MPaOuter Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178
 168 MPaDIN EN ISO 178
Flexural Modulus 4000 MPaDIN EN ISO 178
Flexural Strain at Yield 6.3 %DIN EN ISO 178
Compressive Strain at Break 6.9 %Nominal Compressive Strain at Compressive Strength; DIN EN ISO 604
Compressive Strain at Yield 3.2 %Nominal; DIN EN ISO 604
Compressive Yield Strength 120 MPaElastic Limit
Compressive Strength 58.0 MPa
@Time 3.60e+7 sec
 107 MPa
@Time 360000 sec
 120 MPa
@Time 36.0 sec
 32.0 MPa
@Strain 3.5 %
DIN EN ISO 604
Compressive Modulus 4270 MPaDIN EN ISO 604
Fatigue Strength 60.0 MPa
@# of Cycles 1.00e+6
1 Hz
K Factor (ISO) 5.3 µm/km
@Temperature 200 °C
 6.6 µm/km
@Temperature 240 °C
 8.9 µm/km
@Temperature 100 °C
 11.5 µm/km
@Temperature 20.0 °C
Charpy Impact Unnotched NBEN ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²EN ISO 179/1eA
Coefficient of Friction, Dynamic 0.060
@Temperature 100 °C
Dry Operation
 0.070
@Temperature 20.0 °C
Dry Operation
Coefficient of Friction, Static 0.090
@Temperature 20.0 °C
Dry Operation
Tensile Creep Modulus, 1000 hours 4300 MPaAt 1% Deformation; DIN 53444
Limiting Pressure Velocity 0.16666 MPa-m/secv = 100m/min
 0.1667 MPa-m/secv = 200m/min
 0.31866 MPa-m/secv = 1m/min
 0.480 MPa-m/secv = 10m/min
Compression Set 8.8 %Elastic Compression Limit
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+16 ohm-cmIEC 93
Surface Resistance 2.80e+12 ohmIEC 93
Dielectric Constant 3.2
@Frequency 110 Hz
IEC 250
Dielectric Strength 22.5 kV/mmIEC 243
Dissipation Factor 0.0030IEC 112
 0.052
@Frequency 110 Hz
Comparative Tracking Index 150 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 51.0 µm/m-°C
@Temperature <=100 °C
ISO E 830
 59.0 µm/m-°C
@Temperature <=150 °C
ISO E 831
Specific Heat Capacity 1.35 J/g-°CDSC
Thermal Conductivity 0.250 W/m-KDIN 52612
Melting Point 340 °CDSC
Maximum Service Temperature, Air 100 °CPressed Bushings
 250 °CContinuous
 260 °CShort Term (3h)
Deflection Temperature at 1.8 MPa (264 psi) 160 °CDIN EN ISO 75
Glass Transition Temp, Tg 146 °CDSC
Flammability, UL94 V-0
Oxygen Index 35 %DIN EN ISO 4589
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Alignment Adjustment4Nominal Scale: 1, low; 10, high
Chemical Sterilization10Nominal Scale: 1, low; 10, high
ColorBeige
Creep Resistance6Nominal Scale: 1, low; 10, high
Dimensional Stability with Thermal Expansion6Nominal Scale: 1, low; 10, high
Free from PTFEApplicable
Free from SiliconApplicable
Gamma-rays Radiation Sterilization10Nominal Scale: 1, low; 10, high
High Precision Bushings (negative clearance)Applicable
Injection Molded PartsApplicable
Machined PartsApplicable
Moist Heat Sterilization10Nominal Scale: 1, low; 10, high
Plastic GranulesApplicable
Resistance Against dust, Dirt, Abrasive Substances7Nominal Scale: 1, low; 10, high
Resistance Against Hot Water200
Resistance to Chemicals9Nominal Scale: 1, low; 10, high
Resistant Against DisinfectantApplicable
Rods up to Øe (de)Applicable
ROHS/WEEEApplicable
Sheets up to Maximum ThicknessApplicable
Sliding Velocity40
Suitable for Outdoor Use6Nominal Scale: 1, low; 10, high
Suitable for Use in WaterApplicable
Suitable for VacuumApplicable
Tubes (hollow rods) up to Øe (de)Applicable
UV Rays Resistance9Nominal Scale: 1, low; 10, high
UV-Sterilization7Nominal Scale: 1, low; 10, high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced
AISI 1020 Steel, normalized at 925°C (1700°F), air cooled, 25 mm (1 in.) round
AISI 1020 Steel, normalized at 925°C (1700°F), air cooled, 100 mm (4 in.) round

PZEDEX05 / 122120

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.