MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nylon

(Viewing data as-entered. Click here to return)
Nylacast Nylube GF Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber/Solid Lube Filled

Material Notes: For applications requiring higher compressive strength the NYLUBE GF masterbatch incorporates hollow glass ovule, designed to float and evenly distribute through the polymerising polymer. The glass additive allows the material to operate at higher maximum service temperatures while the wax counteracts the deteriorating surface slip characteristics making this product an outstanding abrasion and temperature resistant material at high loads.

Information provided by Nylacast Ltd.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccmethod A; ISO 1183:1987
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 70.0 MPaType 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 10 %Type 1B, 50mm/min; ISO 527-1/2:1993
Tensile Modulus 3000 MPaType 1B, 50mm/min; ISO 527-1/2:1993
Flexural Strength 115 MPa1.5mm/min; ISO 178:2001
Flexural Modulus 3000 MPa1.5mm/min; ISO 178:2001
Compressive Strength 105 MPaType B, 5mm/min; ISO 604:2002
Compressive Modulus 3000 MPaType B, 5mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 4.50 kJ/m²Type A; ISO 180:2000
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093:1980-01
Surface Resistance 1.00e+12 ohmIEC 60093:1980-01
Dielectric Constant 3.7
@Frequency 1e+6 Hz
IEC 60250:1969-01
 4.0
@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mmIEC 60243-1:1998-01
Comparative Tracking Index 600 VIEC 60112:2003-01
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-2:1999
Melting Point 220 °C
Maximum Service Temperature, Air 190 °CIntermittent
 120 °C
@Time 1.80e+7 sec
Continuous
Minimum Service Temperature, Air -100 °CIntermittent
 -40.0 °CContinuous
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled
Nylacast Nylube Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant)

PNYLAC08 / 89266

Nylon

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.