MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Reynolds EpoxAcoat® HT Thixotropic epoxy gel coat
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Overview: EpoxAcoat® HT is a slightly thixotropic epoxy gel coat that offers high heat resistance (post cure required). Cured epoxy is tough and offers exceptional abrasion resistance. This surface coat will wet out well over a variety of surfaces with good sag resistance. Applications include laminating, precision tooling, master and pattern making, core boxes and fixtures. Use as a surface coat for EpoxAmite® HT high temperature laminating epoxy.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D2240
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 56.0 °C133 °FHeat Deflection Temperature
 140 °C284 °FDeflection Temp. With Post Cure
 
Processing PropertiesMetricEnglishComments
Cure Time 75.0 min1.25 hourThin Film Working Time
 240 min4.00 hourThin Film Tacky Recoat Time
 1440 min24.0 hour
Pot Life 40.0 min40.0 min
 
Descriptive Properties
ColorDark Red
Mix Ratio100A:18Bby weight
Mixed ViscosityLight-paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN294 / 296995

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.