MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Saint-Gobain Tygon® Tygoprene® XL-60 Pump Tubing Formulation
Categories: Polymer; Thermoplastic

Material Notes: Designed specifically for use in peristaltic pump applications, Tygoprene® Pump Tubing maintains a pump life of over 500 hours. It is extremely flexible and exhibits superior flex life, reducing downtime due to pump tubing failure. Tygoprene® Pump Tubing is translucent in color and has excellent chemical resistance to a wide range of fluids, including acids and bases. It can be considered an alternative to silicones and PVC when longer pump life is required.

Features and Benefits

  • Long flex life in peristaltic pumps
  • Low extractables
  • Alternative to PVC
  • Temperature resistant up to 250°F
  • Meets FDA and NSF 51 criteria.

Unless otherwise noted, all tests were conducted at room temperature. Values shown were determined on 1.9 mm thick extruded strip or 1.9 mm thick molded ASTM plaques or molded ASTM durometer buttons.

Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792-00
Water Absorption 0.070 %
@Temperature 22.8 °C,
Time 86400 sec
0.070 %
@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570-98
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 60
@Time 15.0 sec
60
@Time 0.00417 hour
ASTM D2240-03
Tensile Strength 11.2 MPa1630 psiASTM D412-98
Elongation at Break 770 %770 %ASTM D412-98
100% Modulus 3.83 MPa
@Strain 100 %
555 psi
@Strain 100 %
ASTM D412-98
Tear Strength 33.3 kN/m190 pliASTM D1004-03
Compression Set 55 %
@Temperature 70.0 °C,
Time 79200 sec
55 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395-03 Method B
Tensile Set 100 %100 %ASTM D412-98
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 21.7 kV/mm550 kV/inASTM D149-97
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Brittleness Temperature -66.1 °C-87.0 °FASTM D746-98
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
NSF YesYes
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® 2375 Ultra Chemical Resistant Tubing Formulation
Saint-Gobain Tygon® Chemfluor® Convoflex™ Spiral Designed Tubing Aids in Self-flushing and Cleaning
CHT Group EP QS EPI Engineered Polymers Quick Set Epoxy
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry)
AK Steel 304 Austenitic Stainless steel

PSTGQ909 / 160405

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.