MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beryllium Copper Alloy 10C, UNS C82000 TF00 Temper
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Investment, Permanent Mold, Plaster, and Sand.

Applications: Current carrying parts, contact and switch blades, bushings and bearings, soldering iron and resistance welding tips.

Test specimen: TF00 temper, solution treated at 900-950°C, aged 3 hours at 480°C.

Key Words: BeCu; beryllium copper alloy 10C, CA 820, FED QQ-C-390 (CA820), MIL SPEC MIL-C-19464 (Class I)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.62 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 27
@Temperature 635 °C
hot hardness
 36
@Temperature 600 °C
hot hardness
 51
@Temperature 500 °C
hot hardness
 57
@Temperature 400 °C
hot hardness
 59
@Temperature 300 °C
hot hardness
 60
@Temperature 200 °C
hot hardness
 61
@Temperature 100 °C
hot hardness
 62
@Temperature 35.0 °C
hot hardness
Hardness, Rockwell B 96
Tensile Strength, Ultimate 660 MPa
Tensile Strength, Yield 515 MPa
@Strain 0.2 %
Elongation at Break 6.0 %
Modulus of Elasticity 115 GPa
Poissons Ratio 0.33
Fatigue Strength 125 MPa
@# of Cycles 5.00e+7
rotating beam; Temper Not Reported
Machinability 40 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000359 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.8 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 218 W/m-K
@Temperature 20.0 °C
Melting Point 970 - 1090 °C
Solidus 970 °C
Liquidus 1090 °C
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Solution Temperature 900 - 925 °C
Aging Temperature 480 °C
Casting Temperature 1120 - 1175 °CHeavy castings
 1175 - 1230 °CLight castings
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.10 %
Beryllium, Be 0.45 - 0.80 %
Chromium, Cr <= 0.10 %
Cobalt, Co 2.4 - 2.7 %
Copper, Cu >= 96.8 %
Iron, Fe <= 0.10 %
Lead, Pb <= 0.020 %
Nickel, Ni <= 0.20 %
Silicon, Si <= 0.15 %
Tin, Sn <= 0.10 %
Zinc, Zn <= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Beryllium Copper Alloy 10C, UNS C82000 As-cast
UNS C81400, Copper Casting Alloy
Beryllium Copper Alloy 10C, UNS C82000 Cast and Aged
Beryllium Copper Alloy 10C, UNS C82000 TB00 Temper
Beryllium-Copper Alloy 20C, UNS C82500, As Cast

MC82000b5 / 11870

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.