MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil LD 312.AS Low Density Polyethylene (LDPE), Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: LD 312 resins are 4.6 wt% vinyl acetate copolymer for films with good toughness.  The comonomer content and low melt index of those resins help produce films which exhibit superior impact strength, good heat sealability and good low temperature properties.  

Additive:  antiblock: 4000ppm; slip: 800 ppm; thermal stabilizer: yes. 

Availability: Latin America, North America. 

Applications:  co-extrusion films, freezer film, produce bags, foams, lamination film, form fill and seal packaging, poultry bag, rice bags.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccASTM D1505
Vinyl Acetate Content 4.6 %ExxonMobil Method
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 3600 psiASTM D882
Film Tensile Strength at Yield, TD 3400 psiASTM D882
Film Elongation at Break, MD 170 %ASTM D882
Film Elongation at Break, TD 560 %ASTM D882
Puncture Energy 4.10 in-lbExxonMobil Method
Elmendorf Tear Strength MD 190 gASTM D1922
Elmendorf Tear Strength TD 90 gASTM D1922
Dart Drop Test 200 gASTM D1709A
1% Secant Modulus, MD 20000 psiASTM D882
1% Secant Modulus, TD 24000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 221 °FPeak; ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 8.5 %ASTM D1003
Gloss 66 %@ 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX98875 / 238257

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.