HC205TF is a special nucleated polypropylene homopolymer intended for thermoforming packaging. Its increased crystallization temperature allows reduced cycle time and increased output. Products originating from this grade have excellent transparency and organoleptics as well as a good balance of stiffness and impact strength at ambient temperatures. Cas-No: 9003-07-0Applications: - In line and off line thermoforming
- High transparent trays, cups and containers
- Housewares and thin wall packaging
- Margarine tubs and dairy containers
- Blending with copolymers for lids
- Strapping, stretch tape and monofilaments
Special Features:- Excellent processability
- Reduced cycle time and increased output
- Broad application window
- Consistent shrinkage behavior after forming
- Excellent clarity
- Very good stiffness and impact balance
- High gloss
- Excellent transparency
- Excellent organoleptic properties
Information provided by Borealis AG |