MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Geniosil® GF 98 Silane
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Empirical formula: C7H18N2O4Si

CAS No.: 23843-64-3

Properties: Besides the application of GENIOSIL® GF 98 as an adhesion promoter in formulations and primers, it is also used as a coupling agent for modifying fillers and pigments to enhance dispersibility in organic binders and plastics, and thereby improve mechanical properties (flexural strength, tensile strength, modulus etc.).

Special features: GENIOSIL® GF 98 is an alkoxysilane with an amino functional group. It´s a clear, colorless to light yellowish liquid with a characteristically aromatic odor. The compound reacts with moisture under hydrolysis of the alkoxy groups and forms silanols, which reacts further forming siloxanes. As a bifunctional amine, GENIOSIL® GF 98 can also interact with numerous organic polymers and thus function as a molecular bridge between organic and inorganic substrates.

Application: Important applications of GENIOSIL® GF 98 is the use as an adhesion promoter in sealants, adhesives and coatings, and as a coupling agent for inorganic particles, pigments or fillers.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/cc
@Pressure 0.1013 MPa
Molecular Weight 222.3 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point >= 300 °C
@Pressure 0.1013 MPa
Flash Point 99.0 °C
Ignition Temperature 300 °Cliquids; DIN 51794
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.46
 
Descriptive Properties
Active ingredients>95%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9324 / 204853

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.